Rocksolid Light

Welcome to novaBBS (click a section below)

mail  files  register  newsreader  groups  login

Message-ID:  

news: gotcha


tech / sci.engr.joining.welding / Best TIG Welder For Home Use

SubjectAuthor
* Best TIG Welder For Home Usesheilacorvin298
`* Re: Best TIG Welder For Home Userafeel clark
 `* Re: Best TIG Welder For Home UseMiller Scottish
  `* Re: Best TIG Welder For Home UseSnag
   `* Re: Best TIG Welder For Home UseJim Wilkins
    `- Re: Best TIG Welder For Home UseSnag

1
Best TIG Welder For Home Use

<16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=130&group=sci.engr.joining.welding#130

  copy link   Newsgroups: sci.engr.joining.welding
Followup: sci.engr.joining.welding
Subject: Best TIG Welder For Home Use
From: 0f850390...@example.com (sheilacorvin298)
Sender: sheilacorvin298 <0f8503901d844703eea1acecb7a4938a_2807@example.com>
Newsgroups: sci.engr.joining.welding
Followup-To: sci.engr.joining.welding
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Content-Transfer-Encoding: 8bit
User-Agent: Hermes v1.4
Injection-Info: fcc304c7dbe9e9423a7b6bf47b4c9fce;5e06eb0fffef81f9fb42b002dff74be3
Message-ID: <16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com>
Lines: 20
Path: i2pn2.org!i2pn.org!weretis.net!feeder6.news.weretis.net!4.us.feeder.erje.net!2.eu.feeder.erje.net!feeder.erje.net!news.uzoreto.com!newsfeed.xs4all.nl!newsfeed8.news.xs4all.nl!tr2.eu1.usenetexpress.com!feeder.usenetexpress.com!tr2.iad1.usenetexpress.com!news.newsgroupdirect.com!not-for-mail
Date: Fri, 15 Oct 2021 17:18:05 +0000
NNTP-Posting-Date: Fri, 15 Oct 2021 17:18:05 +0000
X-Received-Bytes: 1417
Organization: NewsgroupDirect
X-Complaints-To: abuse@newsgroupdirect.com
 by: sheilacorvin298 - Fri, 15 Oct 2021 17:18 UTC

Well, are you looking for a tig welder which you can use safely at your home?
Tungsten Inert Gas welding (TIG) is a robust welding process widely applicable
due to its variety to weld many materials. With control of the welding
process, the best home tig welder has the advantage of producing pristine
quality welds. Check out our Best TIG Welder For Home Use review article
before purchasing so that you can get a durable, portable, and easy to operate
TIG welding machine.

These are welders that feature many features and offer strong TIG welding.
They are available at an affordable price. The information will be presented
in one location, so finding it should be relatively straightforward. A review
of the best welding tools for home use is provided below, along with their
advantages and disadvantages.

--
for full context, visit https://www.polytechforum.com/welding/best-tig-welder-for-home-use-54749-.htm

Re: Best TIG Welder For Home Use

<1709fbb280ccf88a$1$2251891$4036de63@news.newsgroupdirect.com>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=273&group=sci.engr.joining.welding#273

  copy link   Newsgroups: sci.engr.joining.welding
From: a6f70cab...@example.com (rafeel clark)
Newsgroups: sci.engr.joining.welding
Subject: Re: Best TIG Welder For Home Use
X-poster: Hermes 2.0
References: int_36_5e06eb0fffef81f9fb42b002dff74be3 <16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com>
In-Reply-To: <16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com>
Content-Transfer-Encoding: 8bit
Injection-Info: 6b4fc0d3e453ddd24dc657c7b551cb88;487ebfa698763d9f01f45f867f81564a
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Lines: 6
Path: i2pn2.org!i2pn.org!usenet.blueworldhosting.com!feed1.usenet.blueworldhosting.com!peer02.iad!feed-me.highwinds-media.com!news.highwinds-media.com!feeder.usenetexpress.com!tr1.iad1.usenetexpress.com!news.newsgroupdirect.com!not-for-mail
Date: Wed, 10 Aug 2022 12:31:21 +0000
NNTP-Posting-Date: Wed, 10 Aug 2022 12:31:21 +0000
Organization: NewsgroupDirect
X-Complaints-To: abuse@newsgroupdirect.com
Message-ID: <1709fbb280ccf88a$1$2251891$4036de63@news.newsgroupdirect.com>
X-Received-Bytes: 1726
 by: rafeel clark - Wed, 10 Aug 2022 12:31 UTC

Do you intend to purchase a tig welder that you can safely employ at home? Tungsten inert gas (TIG) welding is a popular welding method because it can be used to join a variety of materials. Since it has control over the welding process, the finest at-home tig welder has the advantage of producing flawlessly high-quality welds. To make sure you get a TIG welding equipment that is reliable, portable, and easy to use, read our analysis of the Best TIG Welder for Home Use before making a purchase.
These welders contain a range of functions and conduct strong TIG welding. They are easily available and moderately priced. Since the information would be shown, finding it should be simple.

--
For full context, visit https://www.polytechforum.com/welding/best-tig-welder-for-home-use-54749-.htm

Re: Best TIG Welder For Home Use

<175b3e540003b3a7$22$1853841$53d3d9df@news.newsgroupdirect.com>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=352&group=sci.engr.joining.welding#352

  copy link   Newsgroups: sci.engr.joining.welding
From: cbf91927...@example.com (Miller Scottish)
Newsgroups: sci.engr.joining.welding
Subject: Re: Best TIG Welder For Home Use
X-Poster: Hermes 2.0
References: int_36_5e06eb0fffef81f9fb42b002dff74be3 <16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com> <1709fbb280ccf88a$1$2251891$4036de63@news.newsgroupdirect.com>
In-Reply-To: <1709fbb280ccf88a$1$2251891$4036de63@news.newsgroupdirect.com>
Content-Transfer-Encoding: 8bit
Injection-Info: 6b4fc0d3e453ddd24dc657c7b551cb88;2488ebe4d440f79211505a2e52e704d5
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Lines: 7
Path: i2pn2.org!i2pn.org!usenet.blueworldhosting.com!diablo1.usenet.blueworldhosting.com!peer03.iad!feed-me.highwinds-media.com!news.highwinds-media.com!feeder.usenetexpress.com!tr3.iad1.usenetexpress.com!news.newsgroupdirect.com!not-for-mail
Date: Tue, 02 May 2023 06:03:36 +0000
Nntp-Posting-Date: Tue, 02 May 2023 06:03:36 +0000
X-Complaints-To: abuse@newsgroupdirect.com
Organization: NewsgroupDirect
Message-Id: <175b3e540003b3a7$22$1853841$53d3d9df@news.newsgroupdirect.com>
X-Received-Bytes: 1591
 by: Miller Scottish - Tue, 2 May 2023 06:03 UTC

Miller Electric's Multimatic 215 multiprocess welder is a great option for hobbyists and DIYers. This welder is small, compact, and versatile; it may be used for a wide range of welding applications. It supports many types of welding, such as TIG, MIG, stick, and flux-coated.

It also offers a ton of features like an LCD screen, dual voltage support, and variable amperage control. This welder offers excellent value for its price and is ideal for light welding work around the house.

--
For full context, visit https://www.polytechforum.com/welding/best-tig-welder-for-home-use-54749-.htm

Re: Best TIG Welder For Home Use

<u2qtjt$o790$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=354&group=sci.engr.joining.welding#354

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!news.eternal-september.org!.POSTED!not-for-mail
From: Snag_...@msn.com (Snag)
Newsgroups: sci.engr.joining.welding
Subject: Re: Best TIG Welder For Home Use
Date: Tue, 2 May 2023 06:53:31 -0500
Organization: A noiseless patient Spider
Lines: 12
Message-ID: <u2qtjt$o790$1@dont-email.me>
References: <16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com>
<1709fbb280ccf88a$1$2251891$4036de63@news.newsgroupdirect.com>
<175b3e540003b3a7$22$1853841$53d3d9df@news.newsgroupdirect.com>
MIME-Version: 1.0
Content-Type: text/plain; charset=utf-8; format=flowed
Content-Transfer-Encoding: 7bit
Injection-Date: Tue, 2 May 2023 11:53:34 -0000 (UTC)
Injection-Info: dont-email.me; posting-host="d79f89e8876faa2cfc354d0fcd817b1f";
logging-data="793888"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX19ySBxlJcuYK/+4HL8WBcGx7EIO8+8OeM0="
User-Agent: Mozilla/5.0 (Windows NT 6.1; WOW64; rv:60.0) Gecko/20100101
Thunderbird/60.6.1
Cancel-Lock: sha1:iPjEsJMFV5eQu4HaB4QGpR5JTEk=
In-Reply-To: <175b3e540003b3a7$22$1853841$53d3d9df@news.newsgroupdirect.com>
Content-Language: en-US
X-Antivirus: Avast (VPS 230502-0, 5/1/2023), Outbound message
X-Antivirus-Status: Clean
 by: Snag - Tue, 2 May 2023 11:53 UTC

On 5/2/2023 1:03 AM, Miller Scottish wrote:
> Multimatic 215 multiprocess welder

Yeah , and it's only 3200 bucks for one that's set up for TIG . And
it's DC only , so no welding aluminum . I like my Everlast EX 250 - it
doesn't MIG (AC/DC TIG and stick and HF start), but I've got a Lincoln
175HD for that . And all in a thousand bucks cheaper than the blue
machine .
--
Snag
"You can lead a dummy to facts
but you can't make him think."

Re: Best TIG Welder For Home Use

<u2rajp$qf73$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=355&group=sci.engr.joining.welding#355

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!news.eternal-september.org!.POSTED!not-for-mail
From: muratla...@gmail.com (Jim Wilkins)
Newsgroups: sci.engr.joining.welding
Subject: Re: Best TIG Welder For Home Use
Date: Tue, 2 May 2023 11:34:12 -0400
Organization: A noiseless patient Spider
Lines: 2
Message-ID: <u2rajp$qf73$1@dont-email.me>
References: <16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com> <1709fbb280ccf88a$1$2251891$4036de63@news.newsgroupdirect.com> <175b3e540003b3a7$22$1853841$53d3d9df@news.newsgroupdirect.com> <u2qtjt$o790$1@dont-email.me>
MIME-Version: 1.0
Content-Type: text/plain;
format=flowed;
charset="UTF-8";
reply-type=response
Content-Transfer-Encoding: 7bit
Injection-Date: Tue, 2 May 2023 15:35:21 -0000 (UTC)
Injection-Info: dont-email.me; posting-host="0bc0add67b2414606c7aeb421cc02751";
logging-data="867555"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX1/7YBWqxZxKeR60mi6oO8luMzVDlc1BmCM="
Cancel-Lock: sha1:LfyNw9P/ryjbJ2OTG9IQ/KLV/2Q=
X-MimeOLE: Produced By Microsoft MimeOLE V16.4.3505.912
Importance: Normal
In-Reply-To: <u2qtjt$o790$1@dont-email.me>
X-MSMail-Priority: Normal
X-Antivirus: AVG (VPS 230502-2, 5/2/2023), Outbound message
X-Antivirus-Status: Clean
X-Newsreader: Microsoft Windows Live Mail 16.4.3505.912
X-Priority: 3
 by: Jim Wilkins - Tue, 2 May 2023 15:34 UTC

"Snag" wrote in message news:u2qtjt$o790$1@dont-email.me...

On 5/2/2023 1:03 AM, Miller Scottish wrote:
> Multimatic 215 multiprocess welder

Yeah , and it's only 3200 bucks for one that's set up for TIG . And
it's DC only , so no welding aluminum . I like my Everlast EX 250 - it
doesn't MIG (AC/DC TIG and stick and HF start), but I've got a Lincoln
175HD for that . And all in a thousand bucks cheaper than the blue
machine .
Snag

---------------------------

An older AC/DC stick/TIG Lincoln Square Wave 175 does all I need it to. The
newer ones at school have more features but I don't weld any better with
them.

Re: Best TIG Welder For Home Use

<u2rl6t$s569$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=356&group=sci.engr.joining.welding#356

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!news.eternal-september.org!.POSTED!not-for-mail
From: Snag_...@msn.com (Snag)
Newsgroups: sci.engr.joining.welding
Subject: Re: Best TIG Welder For Home Use
Date: Tue, 2 May 2023 13:36:11 -0500
Organization: A noiseless patient Spider
Lines: 30
Message-ID: <u2rl6t$s569$1@dont-email.me>
References: <16ae43d24b3ed9d6$1$1208864$4266daf3@news.newsgroupdirect.com>
<1709fbb280ccf88a$1$2251891$4036de63@news.newsgroupdirect.com>
<175b3e540003b3a7$22$1853841$53d3d9df@news.newsgroupdirect.com>
<u2qtjt$o790$1@dont-email.me> <u2rajp$qf73$1@dont-email.me>
MIME-Version: 1.0
Content-Type: text/plain; charset=utf-8; format=flowed
Content-Transfer-Encoding: 8bit
Injection-Date: Tue, 2 May 2023 18:36:13 -0000 (UTC)
Injection-Info: dont-email.me; posting-host="d79f89e8876faa2cfc354d0fcd817b1f";
logging-data="922825"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX18hgpp4eK4N0bQ0h6zuU4EZR3vCL6nwE60="
User-Agent: Mozilla/5.0 (Windows NT 6.1; WOW64; rv:60.0) Gecko/20100101
Thunderbird/60.6.1
Cancel-Lock: sha1:Eh9fMDc2D5oUBq6zqAr5ihLuIfQ=
Content-Language: en-US
In-Reply-To: <u2rajp$qf73$1@dont-email.me>
X-Antivirus: Avast (VPS 230502-2, 5/2/2023), Outbound message
X-Antivirus-Status: Clean
 by: Snag - Tue, 2 May 2023 18:36 UTC

On 5/2/2023 10:34 AM, Jim Wilkins wrote:
> "Snag"  wrote in message news:u2qtjt$o790$1@dont-email.me...
>
> On 5/2/2023 1:03 AM, Miller Scottish wrote:
>> Multimatic 215 multiprocess welder
>
>   Yeah , and it's only 3200 bucks for one that's set up for TIG . And
> it's DC only , so no welding aluminum . I like my Everlast EX 250 - it
> doesn't MIG (AC/DC TIG and stick and HF start), but I've got a Lincoln
> 175HD for that . And all in a thousand bucks cheaper than the blue
> machine .
> Snag
>
> ---------------------------
>
> An older AC/DC stick/TIG Lincoln Square Wave 175 does all I need it to.
> The newer ones at school have more features but I don't weld any better
> with them.
>

I bought the Everlast strictly for TIG though it will also do stick .
If I want to do stick I just fire up the old tombstone . Rare as that
was before I got the new-to-me MIG box I expect it'll be more rare now .
That welder really is almost brand new , the original owner had a loose
connection on one of the outgoing leads that he couldn't figure out ...
might have had all of an hour or so on it when I got it .
--
Snag
"You can lead a dummy to facts
but you can't make him think."


tech / sci.engr.joining.welding / Best TIG Welder For Home Use

1
server_pubkey.txt

rocksolid light 0.9.81
clearnet tor