tech / sci.engr.joining.welding / Paint on flux for the inside of stainless tube

SubjectAuthor
* Paint on flux for the inside of stainless tubeBob La Londe
+- Re: Paint on flux for the inside of stainless tubeSnag
`- Re: Paint on flux for the inside of stainless tubeSnag

1
Paint on flux for the inside of stainless tube

<so5snf$obs$1@gioia.aioe.org>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=151&group=sci.engr.joining.welding#151

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!aioe.org!8O4CTVvGI43OLyHlA+QjDA.user.46.165.242.75.POSTED!not-for-mail
From: non...@none.com99 (Bob La Londe)
Newsgroups: sci.engr.joining.welding
Subject: Paint on flux for the inside of stainless tube
Date: Tue, 30 Nov 2021 12:06:24 -0700
Organization: Aioe.org NNTP Server
Message-ID: <so5snf$obs$1@gioia.aioe.org>
Mime-Version: 1.0
Content-Type: text/plain; charset=UTF-8; format=flowed
Content-Transfer-Encoding: 7bit
Injection-Info: gioia.aioe.org; logging-data="24956"; posting-host="8O4CTVvGI43OLyHlA+QjDA.user.gioia.aioe.org"; mail-complaints-to="abuse@aioe.org";
User-Agent: Mozilla/5.0 (Windows NT 10.0; Win64; x64; rv:91.0) Gecko/20100101
Thunderbird/91.3.2
X-Antivirus: AVG (VPS 211130-0, 11/29/2021), Outbound message
X-Notice: Filtered by postfilter v. 0.9.2
X-Antivirus-Status: Clean
Content-Language: en-US
 by: Bob La Londe - Tue, 30 Nov 2021 19:06 UTC

Have any of you guys used it? I just heard of it for the first time a
little while ago.

--
This email has been checked for viruses by AVG.
https://www.avg.com

Re: Paint on flux for the inside of stainless tube

<so6619$f5j$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=152&group=sci.engr.joining.welding#152

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!reader02.eternal-september.org!.POSTED!not-for-mail
From: Snag_...@msn.com (Snag)
Newsgroups: sci.engr.joining.welding
Subject: Re: Paint on flux for the inside of stainless tube
Date: Tue, 30 Nov 2021 15:45:15 -0600
Organization: A noiseless patient Spider
Lines: 10
Message-ID: <so6619$f5j$1@dont-email.me>
References: <so5snf$obs$1@gioia.aioe.org>
Mime-Version: 1.0
Content-Type: text/plain; charset=utf-8; format=flowed
Content-Transfer-Encoding: 8bit
Injection-Date: Tue, 30 Nov 2021 21:45:14 -0000 (UTC)
Injection-Info: reader02.eternal-september.org; posting-host="fcec71f2021c416e2b6b31aeaf5bec39";
logging-data="15539"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX19lSH2cweM15Jh7HQB6QnYz+Yl2Kqz+Oo4="
User-Agent: Mozilla/5.0 (Windows NT 6.1; WOW64; rv:60.0) Gecko/20100101
Thunderbird/60.6.1
Cancel-Lock: sha1:31AQO5DtTMEmO0H1BaWLeFXZY6I=
In-Reply-To: <so5snf$obs$1@gioia.aioe.org>
X-Antivirus-Status: Clean
Content-Language: en-US
X-Antivirus: Avast (VPS 211130-0, 11/29/2021), Outbound message
 by: Snag - Tue, 30 Nov 2021 21:45 UTC

On 11/30/2021 1:06 PM, Bob La Londe wrote:
> Have any of you guys used it?  I just heard of it for the first time a
> little while ago.
>

I'll let you know in a week or two . Just ordered some a little while
ago .
--
Snag
Let's Go Brandon !

Re: Paint on flux for the inside of stainless tube

<soe42r$pmu$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=153&group=sci.engr.joining.welding#153

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!reader02.eternal-september.org!.POSTED!not-for-mail
From: Snag_...@msn.com (Snag)
Newsgroups: sci.engr.joining.welding
Subject: Re: Paint on flux for the inside of stainless tube
Date: Fri, 3 Dec 2021 16:01:03 -0600
Organization: A noiseless patient Spider
Lines: 10
Message-ID: <soe42r$pmu$1@dont-email.me>
References: <so5snf$obs$1@gioia.aioe.org>
Mime-Version: 1.0
Content-Type: text/plain; charset=utf-8; format=flowed
Content-Transfer-Encoding: 8bit
Injection-Date: Fri, 3 Dec 2021 22:00:59 -0000 (UTC)
Injection-Info: reader02.eternal-september.org; posting-host="cbff919c1f9780bfecb345b4ab5aae34";
logging-data="26334"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX18yxzdAiSvo00HXqsmnlbfkehhIOiBXhGU="
User-Agent: Mozilla/5.0 (Windows NT 6.1; WOW64; rv:60.0) Gecko/20100101
Thunderbird/60.6.1
Cancel-Lock: sha1:9KgMLOwB9dL0ifDjnkDZW+rI0ro=
In-Reply-To: <so5snf$obs$1@gioia.aioe.org>
X-Antivirus-Status: Clean
Content-Language: en-US
X-Antivirus: Avast (VPS 211203-8, 12/3/2021), Outbound message
 by: Snag - Fri, 3 Dec 2021 22:01 UTC

On 11/30/2021 1:06 PM, Bob La Londe wrote:
> Have any of you guys used it?  I just heard of it for the first time a
> little while ago.
>

It came in today's mail , I'll be trying it out tomorrow afternoon .
Letcha know !
--
Snag