Rocksolid Light

Welcome to novaBBS (click a section below)

mail  files  register  newsreader  groups  login

Message-ID:  

All syllogisms have three parts, therefore this is not a syllogism.


tech / sci.engr.joining.welding / Re: Getting More First Minutes Out of A Flap Disc

SubjectAuthor
* Getting More First Minutes Out of A Flap DiscBob La Londe
+* Re: Getting More First Minutes Out of A Flap DiscDavid Billington
|+* Re: Getting More First Minutes Out of A Flap DiscJim Wilkins
||+- Re: Getting More First Minutes Out of A Flap DiscClifford Heath
||`* Re: Getting More First Minutes Out of A Flap DiscMike Spencer
|| +- Re: Getting More First Minutes Out of A Flap DiscJim Wilkins
|| +* Re: Getting More First Minutes Out of A Flap DiscDavid Billington
|| |`- Re: Getting More First Minutes Out of A Flap DiscJim Wilkins
|| `- Re: Getting More First Minutes Out of A Flap DiscJim Wilkins
|`* Re: Getting More First Minutes Out of A Flap DiscBob La Londe
| `- Re: Getting More First Minutes Out of A Flap DiscDavid Billington
+* Re: Getting More First Minutes Out of A Flap DiscCydrome Leader
|+- Re: Getting More First Minutes Out of A Flap DiscBob La Londe
|`- Re: Getting More First Minutes Out of A Flap DiscDirtcrasher
+* Re: Getting More First Minutes Out of A Flap DiscJim Wilkins
|`* Re: Getting More First Minutes Out of A Flap DiscBob La Londe
| +* Re: Getting More First Minutes Out of A Flap DiscSnag
| |+* Re: Getting More First Minutes Out of A Flap DiscBob La Londe
| ||`- Re: Getting More First Minutes Out of A Flap DiscSnag
| |`- Re: Getting More First Minutes Out of A Flap DiscJim Wilkins
| `- Re: Getting More First Minutes Out of A Flap DiscJim Wilkins
+- Re: Getting More First Minutes Out of A Flap DiscClifford Heath
+* Re: Getting More First Minutes Out of A Flap DiscBob Engelhardt
|+- Re: Getting More First Minutes Out of A Flap DiscRichard Smith
|`- Re: Getting More First Minutes Out of A Flap DiscDirtcrasher
`- Re: Getting More First Minutes Out of A Flap DiscBob La Londe

Pages:12
Re: Getting More First Minutes Out of A Flap Disc

<1794ecd986cc52d1$6042$510491$4266dc33@news.newsgroupdirect.com>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=788&group=sci.engr.joining.welding#788

  copy link   Newsgroups: rec.crafts.metalworking sci.engr.joining.welding
From: 83b08c0a...@example.com (Dirtcrasher)
Newsgroups: rec.crafts.metalworking,sci.engr.joining.welding
Subject: Re: Getting More First Minutes Out of A Flap Disc
X-Poster: Hermes 2.0
References: <t5gles$nd7$1@gioia.aioe.org> <Gi_eK.3233$qMI1.1076@fx96.iad>
In-Reply-To: <Gi_eK.3233$qMI1.1076@fx96.iad>
Content-Transfer-Encoding: 8bit
Injection-Info: 6b4fc0d3e453ddd24dc657c7b551cb88;0bea2da53022c238b4c08e3429f43aa4
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Lines: 5
Path: i2pn2.org!rocksolid2!i2pn.org!weretis.net!feeder6.news.weretis.net!usenet.blueworldhosting.com!diablo1.usenet.blueworldhosting.com!feeder.usenetexpress.com!tr2.iad1.usenetexpress.com!news.newsgroupdirect.com!not-for-mail
Date: Mon, 06 Nov 2023 04:02:58 +0000
Nntp-Posting-Date: Mon, 06 Nov 2023 04:02:58 +0000
X-Received-Bytes: 1052
Organization: NewsgroupDirect
X-Complaints-To: abuse@newsgroupdirect.com
Message-Id: <1794ecd986cc52d1$6042$510491$4266dc33@news.newsgroupdirect.com>
 by: Dirtcrasher - Mon, 6 Nov 2023 04:02 UTC

I have the exact same issue, the edge wears down and the disc stops working. The new material never exposes itself. I've sat down with thin, sharp shears and cut off the old to expose some newer material. I hate tossing away a 4$ item after such a short use...

--
For full context, visit https://www.polytechforum.com/welding/getting-more-first-minutes-out-of-a-flap-disc-1526338-.htm