Solar Flux review

<sool7j$q8$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=154&group=sci.engr.joining.welding#154

  copy link   Newsgroups: rec.crafts.metalworking sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!reader02.eternal-september.org!.POSTED!not-for-mail
From: Snag_...@msn.com (Snag)
Newsgroups: rec.crafts.metalworking,sci.engr.joining.welding
Subject: Solar Flux review
Date: Tue, 7 Dec 2021 15:54:54 -0600
Organization: A noiseless patient Spider
Lines: 15
Message-ID: <sool7j$q8$1@dont-email.me>
Mime-Version: 1.0
Content-Type: text/plain; charset=utf-8; format=flowed
Content-Transfer-Encoding: 7bit
Injection-Date: Tue, 7 Dec 2021 21:54:59 -0000 (UTC)
Injection-Info: reader02.eternal-september.org; posting-host="9600ed88c23756a6adfb126455e31e57";
logging-data="840"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX1+zxNgowVere6A08KIh0Z645COqK789AWE="
User-Agent: Mozilla/5.0 (Windows NT 6.1; WOW64; rv:60.0) Gecko/20100101
Thunderbird/60.6.1
Cancel-Lock: sha1:H59XVmLY43mTm58mD78vmcHOpcw=
X-Antivirus-Status: Clean
Content-Language: en-US
X-Antivirus: Avast (VPS 211207-2, 12/7/2021), Outbound message
X-Mozilla-News-Host: news://reader80.eternal-september.org:119
 by: Snag - Tue, 7 Dec 2021 21:54 UTC

This is the stuff we were discussing a few days ago . I tried it out
just a few minutes ago , and it works as advertised . There is no
sugaring on the back side of the piece of 1 3/4 stainless tube I just
butt welded . Not to say the inside weld is smooth , but that's a
reflection on my lack of skill with a TIG torch . I followed the
directions on the package with one exception , I have no methanol on
hand so I used 95% pure ethanol (generic Everclear) as the solvent . It
mixed easily without lumps , applied easily and dried quickly . It turns
powdery as it dries and is easily wiped from the edges you're welding
.. Leaves a black glassy coating that they say is easily removed - I
didn't try .
I give this product 5 stars .
--
Snag
Let's Go Brandon !

Re: Solar Flux review

<soqqln$to8$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=155&group=sci.engr.joining.welding#155

  copy link   Newsgroups: rec.crafts.metalworking sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!reader02.eternal-september.org!.POSTED!not-for-mail
From: djb...@invalid.com (David Billington)
Newsgroups: rec.crafts.metalworking,sci.engr.joining.welding
Subject: Re: Solar Flux review
Date: Wed, 8 Dec 2021 17:40:07 +0000
Organization: A noiseless patient Spider
Lines: 20
Message-ID: <soqqln$to8$1@dont-email.me>
References: <sool7j$q8$1@dont-email.me>
Mime-Version: 1.0
Content-Type: text/plain; charset=utf-8; format=flowed
Content-Transfer-Encoding: 8bit
Injection-Date: Wed, 8 Dec 2021 17:40:07 -0000 (UTC)
Injection-Info: reader02.eternal-september.org; posting-host="bb2246f7910e838d62b90dd66e285d58";
logging-data="30472"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX18S5dEFYMQBA+dyUOniFsKltckbua8sQkU="
User-Agent: Mozilla/5.0 (X11; Linux x86_64; rv:68.0) Gecko/20100101
Thunderbird/68.10.0
Cancel-Lock: sha1:nbSQQPLbhfSOYlTzbEYG2CO25TY=
In-Reply-To: <sool7j$q8$1@dont-email.me>
Content-Language: en-GB
 by: David Billington - Wed, 8 Dec 2021 17:40 UTC

On 07/12/2021 21:54, Snag wrote:
>   This is the stuff we were discussing a few days ago . I tried it out
> just a few minutes ago , and it works as advertised . There is no
> sugaring on the back side of the piece of 1 3/4 stainless tube I just
> butt welded . Not to say the inside weld is smooth , but that's a
> reflection on my lack of skill with a TIG torch . I followed the
> directions on the package with one exception , I have no methanol on
> hand so I used 95% pure ethanol (generic Everclear) as the solvent .
> It mixed easily without lumps , applied easily and dried quickly . It
> turns  powdery as it dries and is easily wiped from the edges you're
> welding . Leaves a black glassy coating that they say is easily
> removed - I didn't try .
>   I give this product 5 stars .

I've just got the SIF purging flux UK equivalent and it also mentions
using washing up liquid and clear varnish as well as methanol to form a
paste, their instructions here
https://www.weldability-sif.com/media/pdfs/info/FO210050.pdf . I haven't
had an opportunity to try it yet.

Re: Solar Flux review

<soqrmc$53d$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=156&group=sci.engr.joining.welding#156

  copy link   Newsgroups: rec.crafts.metalworking sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!reader02.eternal-september.org!.POSTED!not-for-mail
From: Snag_...@msn.com (Snag)
Newsgroups: rec.crafts.metalworking,sci.engr.joining.welding
Subject: Re: Solar Flux review
Date: Wed, 8 Dec 2021 11:57:34 -0600
Organization: A noiseless patient Spider
Lines: 32
Message-ID: <soqrmc$53d$1@dont-email.me>
References: <sool7j$q8$1@dont-email.me> <soqqln$to8$1@dont-email.me>
Mime-Version: 1.0
Content-Type: text/plain; charset=utf-8; format=flowed
Content-Transfer-Encoding: 8bit
Injection-Date: Wed, 8 Dec 2021 17:57:32 -0000 (UTC)
Injection-Info: reader02.eternal-september.org; posting-host="2b9ec5d436b78fd44783128340a6fadd";
logging-data="5229"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX19Sf8oB73wzioR77A34dVSPIhevihCX1Yw="
User-Agent: Mozilla/5.0 (Windows NT 6.1; WOW64; rv:60.0) Gecko/20100101
Thunderbird/60.6.1
Cancel-Lock: sha1:lbuPlud+IIhrf3vNgV0oWJziIBQ=
In-Reply-To: <soqqln$to8$1@dont-email.me>
X-Antivirus-Status: Clean
Content-Language: en-US
X-Antivirus: Avast (VPS 211208-4, 12/8/2021), Outbound message
 by: Snag - Wed, 8 Dec 2021 17:57 UTC

On 12/8/2021 11:40 AM, David Billington wrote:
> On 07/12/2021 21:54, Snag wrote:
>>   This is the stuff we were discussing a few days ago . I tried it out
>> just a few minutes ago , and it works as advertised . There is no
>> sugaring on the back side of the piece of 1 3/4 stainless tube I just
>> butt welded . Not to say the inside weld is smooth , but that's a
>> reflection on my lack of skill with a TIG torch . I followed the
>> directions on the package with one exception , I have no methanol on
>> hand so I used 95% pure ethanol (generic Everclear) as the solvent .
>> It mixed easily without lumps , applied easily and dried quickly . It
>> turns  powdery as it dries and is easily wiped from the edges you're
>> welding . Leaves a black glassy coating that they say is easily
>> removed - I didn't try .
>>   I give this product 5 stars .
>
> I've just got the SIF purging flux UK equivalent and it also mentions
> using washing up liquid and clear varnish as well as methanol to form a
> paste, their instructions here
> https://www.weldability-sif.com/media/pdfs/info/FO210050.pdf . I haven't
> had an opportunity to try it yet.
>

Looking at their instructions it appears this flux is water soluble
after welding . That seems to be the major difference . I got the stuff
because I'm building an exhaust system for my truck and I didn't want to
have to purge with gas . Most of the welding will be on the bench (so to
speak) but some joints will have to be welded on the truck . I'm still
hoping that I can figure out the MIG for those , but they will still
need some shielding on the back side .
--